Engineering the Palladium–WSe 2 Interface Chemistry for Field Effect Transistors with High-Performance Hole Contacts
Data di pubblicazione: 7 Dic 2018
Palladium has been widely employed as a hole contact to WSe 2 and has enabled, at times, the highest WSe 2 transistor performance. However, there are orders of magnitude variation across the literature in Pd–WSe 2 contact resistance and I ON / I OFF ratios with no true understanding of how to consistently achieve high-performance contacts. In this work, WSe 2 transistors with impressive I ON / I OFF ratios of 10 6 and Pd–WSe 2 Schottky diodes with near-zero variability are demonstrated utilizing Ohmic-like Pd contacts through deliberate control of the interface chemistry. The increased concentration of a PdSe x intermetallic is correlated with an Ohmic band alignment and concomitant defect passivation, which further reduces the contact resistance, variability, and barrier height inhomogeneity. The lowest contact resistance occurs when a 60 min post-metallization anneal at 400 °C in forming gas (FG) is performed. X-ray photoelectron spectroscopy indicates this FG anneal produces 3× the concentration of PdSe x and an Ohmic band alignment, in contrast to that detected after annealing in ultrahigh vacuum, during which a 0.2 eV hole Schottky barrier forms. Raman spectroscopy and scanning transmission electron microscopy highlight the necessity of the fabrication step to achieve high-performance contacts as no PdSe x forms, and WSe 2 is unperturbed by room temperature Pd deposition. However, at least one WSe 2 layer is consumed by the necessary interface reactions that form PdSe x requiring strategic exploitation of a sacrificial WSe 2 layer during device fabrication. The interface chemistry and structural properties are correlated with Pd–WSe 2 diode and transistor performance, and the recommended processing steps are provided to enable reliable high-performance contact formation.